Inconel 188 /Alloy 188 /UNS R30188 Cobalt Base Superalloy

Inconel 188 /Alloy 188 /UNS R30188 Cobalt Base Superalloy

Inconel 188 /Alloy 188 /UNS R30188 Cobalt Base Superalloy

Product Details:

Place of Origin: Suzhou, China
Brand Name: AIWEN
Certification: SH
Model Number: SH-Alloy 188

Payment & Shipping Terms:

Minimum Order Quantity: 50KG
Price: Available per request
Packaging Details: By customers' require
Delivery Time: 30-40days
Payment Terms: T/T
Supply Ability: 10000 KG per month
Contact Now
Detailed Product Description

Inconel 188 /Alloy 188 /UNS R30188 Cobalt Base Superalloy

Specifications of Inconel 188 /Alloy 188 /UNS R30188 Cobalt Base Superalloy:

AMS 5608, AMS 5801
EN 2.4683
PWA 1042
UNS R30188
Werkstoff 2.4683

Features of Inconel 188 /Alloy 188 /UNS R30188 Cobalt Base Superalloy:

Strength and oxidation resistant to 2000°F
Good post-aging ductility
Resistant to sulfate deposit hot corrosion

Applications of Inconel 188 /Alloy 188 /UNS R30188 Cobalt Base Superalloy:

Gas turbine engine combustor cans
Spray bars
Flame-holders and afterburner liners